The Physical Properties Of Aluminium-7xxx Series Alloys Produced By Powder Metallurgy Method

A. Acar, A. K. Ekşi, A. Ekicibil
Published 2018 · Engineering

Cite This
Download PDF
Analyze on Scholarcy
Share
Alumix-431 materials   were prepared by cold and warm compaction method applying 350-400 MPa pressures at RT (room temperature) 50 and 80°C temperatures.  The density measurements of materials were performed; the thermoelectric properties of materials were investigated at 5-300K under the He atmosphere, and the relationship between the measurements and sample properties was examined. The measurements of thermoelectric properties showed that maximum resistivity [Alumix -431-1] and thermal conductivity [Alumix -431-6] values were obtained 0.161Ωm and 24.31W/Km, respectively at 285-295K temperature ranges and minimum electrical resistivity and thermal conductivity values  were obtained on Alumix-431-6 and Alumix-431-1 samples, respectively. It was observed that Seebeck coefficient values varied mostly from negative sign to positive sign indicated dominate from carriers.  The maximum Figure of merit value was determined as 18.71×10 -2 ; on the Alumix-431-5 alloy at 96.904K
This paper references
10.1142/6703
Annual review of nano research
G. Cao (2008)
Warm compaction of aluminium alloy Alumix 123
Lubos Meluch (2010)
10.1016/J.COMPOSITESB.2011.09.004
Effect of lubricants on warm compaction process of Cu-based composite
S. S. Feng (2012)
10.1016/j.msea.2009.05.039
Metallurgical assessment of an emerging Al–Zn–Mg–Cu P/M alloy
A.D.P. LaDelpha (2009)
10.1016/J.MATDES.2013.12.024
Effect of cooling aging on microstructure and mechanical properties of an Al–Zn–Mg–Cu alloy
Yan Liu (2014)
10.1016/J.SOLIDSTATESCIENCES.2010.06.005
Effects of silicon addition on thermoelectric properties of bulk Zn4Sb3 at low-temperatures
Lei Pan (2010)
10.1016/J.RSER.2013.10.027
A review on thermoelectric renewable energy: Principle parameters that affect their performance
M. Elsheikh (2014)
10.1016/J.MATCHEMPHYS.2012.10.009
Investigation of Al substitution on the thermoelectric properties of SrSi2
Yung-Kang Kuo (2012)
10.1088/2053-1591/1/3/035901
Thermoelectric properties of n-type Bi2Te2.7Se0.3 with addition of nano-ZnO:Al particles
Shaowei Song (2014)
10.1016/J.CERAMINT.2009.04.010
Characterization of Al-doped ZnO thermoelectric materials prepared by RF plasma powder processing and hot press sintering
Henrich Cheng (2009)
10.1016/S0921-5093(01)01771-3
Pre-precipitation study in the 7012 Al–Zn–Mg–Cu alloy by electrical resistivity
R. Ferragut (2002)
10.1179/1743290112Y.0000000047
Experimental study and predictive modelling of cold compaction green density in powder metallurgy of stainless steel components
Elham Jafar-Salehi (2013)
10.1016/1044-5803(96)00002-2
Thermoelectric power characterization of a 2024 aluminum alloy during solution treatment and aging
D. Sun (1996)
Material science and engineering : an introduction
W. D. Callister (1985)
10.1016/J.JALLCOM.2006.05.026
Electrical, magnetic, thermal and thermoelectric properties of the bergman phase Mg32(Al,Zn)49 complex metallic alloy
A. Smontara (2007)
AA 2014 ALAŞIMINDA PRESLEME VE SİNTERLEMENİN GÖZENEK MORFOLOJİSİ VE MİKROYAPISAL ÖZELLİKLERE ETKİLERİ
Hakan Gökmeşe (2013)
10.1016/J.MATCHAR.2013.02.004
Fabrication and microstructural characterization of Al/Zn-enriched layers on pure magnesium
R. Móla (2013)
G.J.,‘’Ca3AlSb3: An inexpensive, nontoxic thermoelectric material for waste heat recovery‘
A. Zevalkink (2011)
10.1007/S13369-014-1432-9
Characteristics of Al–Zn–Mg–Cu Alloys with Nickel Additives Synthesized via Mechanical Alloying, Cold Compaction, and Heat Treatment
H. Naeem (2014)
10.1016/J.MSEA.2004.09.013
On the nature of T(Al2Mg3Zn3) and S(Al2CuMg) phases present in as-cast and annealed 7055 aluminum alloy
C. Mondal (2005)
10.1016/J.SSC.2005.11.040
Degradation of superconducting properties in MgB2 by Cu addition
M. Aksan (2006)
10.1088/1742-6596/150/1/012044
Influence of the sample mounting on thermal conductance measurements using PPMS TTO option
James J. Sebek (2009)
10.1080/09500839.2013.813981
Thermoelectric power in low-density interstitial-free iron-aluminium alloys
Radhakanta Rana (2013)
Thermoelectric properties of Al-doped Mg 2Si 1- x Sn x ( x ? 0.1)
Jun-ichi Tani (2008)
10.1016/J.CRYOGENICS.2013.12.008
Low temperature thermal conductivity of aluminum alloy 5056
Bertrand Baudouy (2014)
10.1002/CHIN.200849218
Recent Progress in Oxide Thermoelectric Materials: p-Type Ca3Co4O9 and n-Type SrTiO3-
H. Ohta (2008)
10.5402/2012/580659
Thermal Conductivity of Cu-Cr-Zr-Ti Alloy in the Temperature Range of 300-873K
S. Chenna Krishna (2012)
‘ ’ Thermoelectric properties of Al - doped Mg 2 Si 1x Sn x [ x ≤ 0 . 1 ]
H. Kido
10.1016/J.JMMM.2006.12.022
Effect of warm compaction on the magnetic and electrical properties of Fe-based soft magnetic composites
H. Shokrollahi (2007)
10.4028/www.scientific.net/MSF.794-796.501
Mechanical Properties of Sintered of Al-5.5Zn-2.5Mg-0.5Cu PM Alloy
Haris Rudianto (2014)
10.1016/j.matdes.2008.10.008
An approach for the aging process optimization of Al–Zn–Mg–Cu series alloys
Shenqing Fang (2009)
10.1103/PHYSREVB.72.115120
Electrical transport, thermal transport, and elastic properties of M2AlC (M=Ti, Cr, Nb, and V)
J. Hettinger (2005)
Corrosion behaviour and galvanic studies of microscopic oxidation films on Al - Zn - Mg - Cu alloy ‘
W. Xue
Thermoelectric properties of hot-pressed Aland Co-doped ıron disilicide materials‘
Z. He (2007)
10.1038/nmat2090
Complex thermoelectric materials.
G. Snyder (2008)
10.1016/j.jallcom.2008.10.115
Microstructural development of spray-deposited Al–Zn–Mg–Cu alloy during subsequent processing
Feng Wang (2009)
H.,‘’Thermoelectric properties of Aldoped Mg2Si1-xSnx[x≤0.1]‘
Tani J.-I (2018)
10.1016/J.ENCONMAN.2009.09.030
New method for investigation of parameters of real thermoelectric modules
Rasit Ahiska (2010)
10.1080/10739140802584772
Analysis of a New Method for Measurement of Parameters of Real Thermoelectric Module Employed in Medical Cooler for Renal Hypothermia
Rasit Ahiska (2009)
10.1016/J.MATDES.2010.06.013
Investigation on the effect of lubrication and forming parameters to the green compact generated from iron powder through warm forming route
Mujibur Rahman (2011)
10.7763/IJCEA.2012.V3.154
Effects of Particle Size Distribution and Packing Characteristics on the Preparation of Highly-Loaded Coal-Water Slurry
Patnaree Buranasrisak (2012)
10.1515/AMM-2015-0136
Effect Of SiC Particles On Sinterability Of Al-Zn-Mg-Cu P/M Alloy
Haris Rudianto (2015)
10.1016/J.JALLCOM.2013.06.055
Microstructure evolution and mechanical properties of Al-Zn-Mg-Cu alloy reprocessed by spray-forming and heat treated at peak aged condition
E. M. Mazzer (2013)
THE INFLUENCE OF SINTERING AND SHOT PEENING PROCESSES ON ALUMIX 431 POWDER MATERIALS
Makine Mühendisliği (2010)
10.1155/2015/987687
Evaluation of Sintering Behavior of Premix Al-Zn-Mg-Cu Alloy Powder
Haris Rudianto (2015)
Corrosion behaviour and galvanic studies of microscopic oxidation films on Al-Zn-Mg-Cu alloy‘’, Surface ad Coatings Technology
W. Xue (2018)
Thermoelectric properties of hot-pressed Aland Co-doped ıron disilicide materials‘
Z. He (2007)
10.1007/S11661-007-9153-2
The Effect of Particle Shape on the Sintering of Aluminum
Z. Liu (2007)
10.1016/S1359-6454(00)00085-9
Correlation between the microstructural evolution of a 6061 aluminium alloy and the evolution of its thermoelectric power
V. Massardier (2000)
10.1016/J.MATDES.2012.03.049
Influence of second phases on mechanical properties of spray-deposited Al–Zn–Mg–Cu alloy
Yandong Jia (2012)
10.1016/J.JALLCOM.2010.10.021
Microstructural behavior of the heat treated n-type 95% Bi2Te3–5% Bi2Se3 gas atomized thermoelectric powders
Mahedi Hasan Bhuiyan (2011)
New Method for Investigation of Dynamic Parameters of Thermoelectric Modules
Rasit Ahiska (2007)
10.1016/S1359-6454(96)00033-X
Precipitation kinetics, mechanical strength and electrical conductivity of AlZnMgCu alloys
P. Guyot (1996)
10.1039/C4EE01320D
Measuring thermoelectric transport properties of materials
K. Borup (2015)
Ca 3 AlSb 3 : an inexpensive , non-toxic thermoelectric material for waste heat recovery
Alex Zevalkink (2011)
10.1016/J.MATDES.2010.05.058
Powder material parameters establishment through warm forming route
Mujibur Rahman (2011)
10.1016/J.MATCHEMPHYS.2007.06.028
Structural characterization and transport properties of the HTc Bi2Sr2(Ca,Cd)Cu2O8+δ glass-ceramic rods
M. Aksan (2007)
10.4028/www.scientific.net/MSF.519-521.853
Correlation of Strength with Hardness and Electrical Conductivity for Aluminium Alloy 7010
M. A. Salazar-Guapuriche (2006)
10.1179/003258904225015392
Tensile and fatigue properties of cold and warm compacted Alumix 431 alloy
A. K. Ekşi (2004)
10.1016/0038-1098(95)00176-X
On thermally activated electrical resistivity in metallic glasses
Mushtaq Ahmed Gormani (1995)



This paper is referenced by
Semantic Scholar Logo Some data provided by SemanticScholar